Graphite crucible is a crucible made of graphite, silicon carbide, clay, silica, wax stone, pitch and tar, etc. fired as raw materials. The material used for graphite crucible is made of high purity, high strength and high density graphite refractory material, which can be made into graphite crucible, graphite casting crucible and graphite oil tank through CNC processing.
Features of Kerui Graphite Crucible
- Good thermal stability of graphite crucible: special formula for the use conditions of graphite crucible of rapid heat and cold.
- Good corrosion resistance and impact resistance of graphite crucible to ensure the reliability of product quality.
- Good resistance to strong acid and alkali of graphite crucible.
- Good heat conduction performance of graphite crucible: it can greatly shorten the melting time and save energy.
- The ash content of graphite crucible is less than 300pp to ensure that the precious metals are not polluted in smelting.
Application of Kerui Graphite Crucible
흑연 도가니는 주로 자색 구리, 황동, 금, 은, 아연, 납 및 그 합금과 같은 비철금속을 녹이는 데 사용됩니다.
참고.
- Storage: place in a dry place, not wet.
- Handling: Handle with care and do not collide.
- Placement: Use the correct crucible holder and make sure that the crucible base is firmly in contact.
- Charging: Fill the crucible with ingots or scrap metal carefully, do not squeeze hard and do not insert and squeeze too closely.
- Adding melt: Use as little melt as possible.
- Cleaning: Keep the crucible clean, pour out the residual metal quickly at the end of the operation and remove the residue carefully.
- Drying and preheating: If the crucible is damp, it needs to be dried slowly at a temperature below 100 °C.
- Water removal: Remove all water around the furnace to avoid leakage causing metal and water contact to fry.
표준 흑연 도가니 사양.
모델 | 상단 포트 외경 ±2% | 두께 | 하단 외경 ±2% | 높이 ±2% |
1# | 67 | 8± 1.0 | 35 | 65 |
1.5# | 78 | 10± 1.0 | 60 | 80 |
2# | 88 | 10± 1.0 | 62 | 100 |
3# | 100 | 12± 1.0 | 75 | 115 |
4# | 115 | 12± 1.0 | 85 | 115 |
5# | 122 | 13± 1.0 | 85 | 138 |
6# | 125 | 14 ± 1.0 | 85 | 155 |
41# | 215 | 19~ 21.5 | 150 | 290 |
45# | 250 | 19~ 21.5 | 180 | 295 |
70# | 285 | 19~ 21.5 | 215 | 245 |
80# | 310 | 20~ 22.5 | 210 | 370 |
90# | 320 | 21~ 23.5 | 230 | 385 |
100# | 314 | 21~ 23.5 | 220 | 408 |
200# | 400 | 23~ 25.5 | 290 | 475 |
260# | 416 | 24~ 26.5 | 250 | 585 |
300# | 452 | 26~ 29 | 310 | 580 |
360# | 462 | 28~ 31 | 342 | 674 |
390# | 530 | 28~ 31 | 410 | 560 |
400# | 515 | 29~ 32 | 340 | 600 |
420# | 515 | 29~ 32 | 330 | 673 |
440# | 620 | 29~ 32 | 340 | 500 |
450# | 516 | 32~ 35 | 340 | 710 |
530# | 580 | 31~ 34 | 330 | 635 |
560# | 590 | 33~ 36 | 330 | 690 |
570# | 620 | 33~ 36 | 335 | 570 |
580# | 545 | 33~ 36 | 317 | 750 |
610# | 607 | 34~ 38 | 350 | 630 |
680# | 585 | 34~ 38 | 330 | 760 |
690# | 600 | 34~ 38 | 330 | 805 |
700# | 615 | 34~ 38 | 350 | 758 |
840# | 700 | 35~ 39 | 470 | 675 |
950# | 720 | 37~ 41 | 300 | 740 |
970# | 720 | 34~ 38 | 470 | 730 |
1100# | 715 | 35~ 39 | 478 | 846 |
1150# | 855 | 42~ 46 | 340 | 677 |
1200# | 780 | 36~ 40 | 450 | 752 |
1250# | 725 | 36~ 40 | 470 | 905 |
1500# | 784 | 37~ 41 | 450 | 890 |
1700# | 778 | 40~ 44 | 442 | 1050 |
2500# | 880 | 44~ 48 | 350 | 1150 |
참고: 표준형 흑연 도가니 사양은 국가 표준 GB/T 26279-2010을 참조하세요.
Parameters of Kerui Graphite Crucible
항목 | Ⅰ | Ⅱ | 테스트 방법 | ||
형성 방법 | 가소성(S) | 등방성 압력(D) | 가소성(S) | 등방성 압력(D) | |
탄소 함량 /% | ≥ 38 | ≥ 45 | ≥ 38 | ≥ 45 | GB/T 1655-2008 |
벌크 밀도 /(g/cm3) | ≥ 1.70 | ≥ 1.85 | ≥ 1.70 | ≥ 1.85 | GB/T 2997-2000 |
다공성 /% | ≤ 29 | ≤ 21 | ≤ 29 | ≤ 21 | GB/T 2997-2000 |
상온 압축 강도 /MPa | ≥ 20 | ≥ 25 | ≥ 20 | ≥ 25 | GB/T 5072.2-2004 |
내화성 / ℃ | ≥ 1500 | ≥ 1500 | ≥ 1400 | ≥ 1400 | GB/T 7322-2007; 항산화 글레이즈 코팅 |